2011-06-06

Modular Walls - QC - Fine cast


A piece of the mould, not something to worry about though.


A few air bubbles, otherwise fine. Finecast.


More bubbles... more problematic ones, though totally solvable with more vacuum and faster pouring.


Overview of front.


Close-up.


Edge.
A fine cast.

2 kommentarer:

  1. That's a bit too much finecast that! So the front was the hardest one to get free of bubbles -- to many bubbles to clean up if we make them in greater quantity.

    I really think that some form of ventsor pits could improve it.

    FoB

    SvaraRadera
  2. Anonym said: " ...blah-blah-blah could improve it."

    This is true. Make these and the casting may commence.

    Regards from Llama, Hater of Hithero

    SvaraRadera